Brand Name: | UNMAG |
MOQ: | 100pcs |
Price: | As negotiation |
Delivery Time: | 20-25days |
Payment Terms: | T/T L/C |
Samarium-Cobalt Alloy Magnets, also known as Samarium Cobalt Magnet, are composed of an alloy of samarium and cobalt. They are widely used in spaceflight, national defense, microwave, sensors and other fields. These magnets have excellent temperature stability, corrosion resistance, and high magnetic properties.
The samarium cobalt magnet has a wide range of grades. Including YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 and other grades. The magnetization of the magnet can be through axial, thickness or customized according to the needs. The samarium cobalt magnets are generally uncoated and have excellent temperature stability and corrosion resistance.
The Samarium Cobalt Magnet has a wide range of applications in the aerospace, automotive, medical and other industries. Its good temperature stability and corrosion resistance make it a good choice for many applications.
Grade | Coating | Operating Temperature | Application | Magnetization | Material |
---|---|---|---|---|---|
YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 | Uncoated | 250-500°C | Spaceflight,National Defense,Microwave,Sensors | Through Axial,Thickness Or Customized | Samarium Cobalt |
Grade | Remanence (Br) |
Coercivity (Hcb) |
Intrinsic Coercivity (Hcj) |
(BH)max
|
Curie Temperature (TC) |
Max Work Temp (TW) |
Temperature Coefficient of Br (Br) |
Temperature Coefficient of Hcj (Hcj) |
|||||
T | kGS | kA/m | KOe | KA/m | KOe | KJ/m3 | MGOe | ℃ | ℃ | %℃ | %℃ | ||
YX-16s | 0.79-0.84 | 7.9-8.4 | 620-660 | 7.8-8.3 | ≥1830 | ≥23 | 118-135 | 15-17 | 750 | 250 | -0.035 | -0.28 | |
YX-18s | 0.84-0.89 | 8.4-8.9 | 660-700 | 8.3-8.8 | ≥1830 | ≥23 | 135-151 | 17-19 | 750 | 250 | -0.040 | -0.28 | |
YX-20s | 0.89-0.93 | 8.9-9.3 | 684-732 | 8.6-9.2 | ≥1830 | ≥23 | 150-167 | 19-21 | 750 | 250 | -0.045 | -0.28 | |
YX-22s | 0.92-0.96 | 9.2-9.6 | 710-756 | 8.9-9.5 | ≥1830 | ≥23 | 167-183 | 21-23 | 750 | 250 | -0.045 | -0.28 | |
YX-24s | 0.96-1.00 | 9.6-10.0 | 740-788 | 9.3-9.9 | ≥1830 | ≥23 | 183-199 | 23-25 | 750 | 250 | -0.045 | -0.28 | |
LTc(YX-10) | 0.62-0.66 | 6.2-6.6 | 485-517 | 6.1-6.5 | ≥1830 | ≥23 | 75-88 | 9.5-11 | 750 | 300 | Temp Range | Br Temp Coefficient%℃ | |
20-100℃ | +0.0156%℃ | ||||||||||||
100-200℃ | +0.0087%℃ | ||||||||||||
200-300℃ | +0.0007%℃ | ||||||||||||
YX-12 | 0.70-0.74 | 7.0-7.4 | 358-390 | 4.5-4.9 | 358-478 | 4.5-6 | 80-103 | 10-13 | 450 | 200 | |||
YXG-24H | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1990 | ≥25 | 175-191 | 22-24 | 800 | 350 | -0.025 | -0.20 | |
YXG-26H | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1990 | ≥25 | 191-207 | 24-26 | 800 | 350 | -0.030 | -0.20 | |
YXG-28H | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1990 | ≥25 | 207-220 | 26-28 | 800 | 350 | -0.035 | -0.20 | |
YXG-30H | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1990 | ≥25 | 220-240 | 28-30 | 800 | 350 | -0.035 | -0.20 | |
YXG-32H | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1990 | ≥25 | 230-255 | 29-32 | 800 | 350 | -0.035 | -0.20 | |
YXG-22 | 0.93-0.97 | 9.3-9.7 | 676-740 | 8.5-9.3 | ≥1433 | ≥18 | 160-183 | 20-23 | 800 | 300 | -0.020 | -0.20 | |
YXG-24 | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1433 | ≥18 | 175-191 | 22-24 | 800 | 300 | -0.025 | -0.20 | |
YXG-26 | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1433 | ≥18 | 191-207 | 24-26 | 800 | 300 | -0.030 | -0.20 | |
YXG-28 | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1433 | ≥18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |
YXG-30 | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1433 | ≥18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |
YXG-32 | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1433 | ≥18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |
YXG-26M | 1.02-1.05 | 10.2-10.5 | 676-780 | 8.5-9.8 | 955-1433 | 12-18 | 191-207 | 24-26 | 800 | 300 | -0.035 | -0.20 | |
YXG-28M | 1.03-1.08 | 10.3-10.8 | 676-796 | 8.5-10.0 | 955-1433 | 12-18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |
YXG-30M | 1.08-1.10 | 10.8-11.0 | 676-835 | 8.5-10.5 | 955-1433 | 12-18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |
YXG-32M | 1.10-1.13 | 11.0-11.3 | 676-852 | 8.5-10.7 | 955-1433 | 12-18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |
YXG-24L | 0.95-1.02 | 9.5-10.2 | 541-716 | 6.8-9.0 | 636-955 | 8-12 | 175-191 | 22-24 | 800 | 250 | -0.025 | -0.20 | |
YXG-26L | 1.02-1.05 | 10.2-10.5 | 541-748 | 6.8-9.4 | 636-955 | 8-12 | 191-207 | 24-26 | 800 | 250 | -0.035 | -0.20 | |
YXG-28L | 1.03-1.08 | 10.3-10.8 | 541-764 | 6.8-9.6 | 636-955 | 8-12 | 207-220 | 26-28 | 800 | 250 | -0.035 | -0.20 | |
YXG-30L | 1.08-1.15 | 10.8-11.5 | 541-796 | 6.8-10.0 | 636-955 | 8-12 | 220-240 | 28-30 | 800 | 250 | -0.035 | -0.20 | |
YXG-32L | 1.10-1.15 | 11.0-11.5 | 541-812 | 6.8-10.2 | 636-955 | 8-12 | 230-255 | 29-32 | 800 | 250 | -0.035 | -0.20 | |
LTC(YXG-22) | 0.94-0.98 | 9.4-9.8 | 668-716 | 8.4-9.0 | ≥1433 | ≥18 | 167-183 | 21-23 | 840 | 300 | Temp Range | Br Temp Coefficient%℃ | |
–50-25℃ | ﹢0.005%℃ | ||||||||||||
20-100℃ | -0.008%℃ | ||||||||||||
100-200℃ | -0.008%℃ | ||||||||||||
200-300℃ | -0.011%℃ |
Parameter Name | Unit | SmCo5 | Sm2Co17 |
Density | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
Curie Temperature | ℃ | 700 ~ 750 | 800 ~ 850 |
Max. Operating Temperature 250 350 | ℃ | 250 | 350 |
Temperature Coefficient Of Br -0.05 -0.03 | %/℃ | -0.05 | -0.03 |
Vickers Hardness 450 ~ 500 550 ~600 | HV | 450 ~ 500 | 550 ~600 |
Electronic Ressistivity | Ω.cm | 5 ~ 6 x 10(-5) | 8 ~ 9 x 10(-5) |
Thermal Conductivity | W/mK | 12 | 13 |
UNMAG Samarium Cobalt Magnets, also known as rare earth magnets, are manufactured in China with Grade YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32. UNMAG Samarium-Cobalt Magnet can be magnetized through axial, thickness or customized as required. Its material is samarium cobalt, and it is uncoated. The delivery time is 25-30 days. It is widely used in spaceflight, national defense, microwave and sensors.
UNMAG is a leading manufacturer of Rare Earth Magnets, including Samarium Cobalt Magnets. Our Samarium Cobalt Magnets are made with the highest quality materials and are expertly crafted to meet your specific requirements. Our Samarium Cobalt Magnets are highly reliable and have a long service life.
For your Samarium Cobalt Magnet needs, trust only UNMAG. Contact us today to get started.
Samarium Cobalt Magnet Packaging and Shipping:
Brand Name: | UNMAG |
MOQ: | 100pcs |
Price: | As negotiation |
Packaging Details: | cartons,pallets |
Payment Terms: | T/T L/C |
Samarium-Cobalt Alloy Magnets, also known as Samarium Cobalt Magnet, are composed of an alloy of samarium and cobalt. They are widely used in spaceflight, national defense, microwave, sensors and other fields. These magnets have excellent temperature stability, corrosion resistance, and high magnetic properties.
The samarium cobalt magnet has a wide range of grades. Including YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 and other grades. The magnetization of the magnet can be through axial, thickness or customized according to the needs. The samarium cobalt magnets are generally uncoated and have excellent temperature stability and corrosion resistance.
The Samarium Cobalt Magnet has a wide range of applications in the aerospace, automotive, medical and other industries. Its good temperature stability and corrosion resistance make it a good choice for many applications.
Grade | Coating | Operating Temperature | Application | Magnetization | Material |
---|---|---|---|---|---|
YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 | Uncoated | 250-500°C | Spaceflight,National Defense,Microwave,Sensors | Through Axial,Thickness Or Customized | Samarium Cobalt |
Grade | Remanence (Br) |
Coercivity (Hcb) |
Intrinsic Coercivity (Hcj) |
(BH)max
|
Curie Temperature (TC) |
Max Work Temp (TW) |
Temperature Coefficient of Br (Br) |
Temperature Coefficient of Hcj (Hcj) |
|||||
T | kGS | kA/m | KOe | KA/m | KOe | KJ/m3 | MGOe | ℃ | ℃ | %℃ | %℃ | ||
YX-16s | 0.79-0.84 | 7.9-8.4 | 620-660 | 7.8-8.3 | ≥1830 | ≥23 | 118-135 | 15-17 | 750 | 250 | -0.035 | -0.28 | |
YX-18s | 0.84-0.89 | 8.4-8.9 | 660-700 | 8.3-8.8 | ≥1830 | ≥23 | 135-151 | 17-19 | 750 | 250 | -0.040 | -0.28 | |
YX-20s | 0.89-0.93 | 8.9-9.3 | 684-732 | 8.6-9.2 | ≥1830 | ≥23 | 150-167 | 19-21 | 750 | 250 | -0.045 | -0.28 | |
YX-22s | 0.92-0.96 | 9.2-9.6 | 710-756 | 8.9-9.5 | ≥1830 | ≥23 | 167-183 | 21-23 | 750 | 250 | -0.045 | -0.28 | |
YX-24s | 0.96-1.00 | 9.6-10.0 | 740-788 | 9.3-9.9 | ≥1830 | ≥23 | 183-199 | 23-25 | 750 | 250 | -0.045 | -0.28 | |
LTc(YX-10) | 0.62-0.66 | 6.2-6.6 | 485-517 | 6.1-6.5 | ≥1830 | ≥23 | 75-88 | 9.5-11 | 750 | 300 | Temp Range | Br Temp Coefficient%℃ | |
20-100℃ | +0.0156%℃ | ||||||||||||
100-200℃ | +0.0087%℃ | ||||||||||||
200-300℃ | +0.0007%℃ | ||||||||||||
YX-12 | 0.70-0.74 | 7.0-7.4 | 358-390 | 4.5-4.9 | 358-478 | 4.5-6 | 80-103 | 10-13 | 450 | 200 | |||
YXG-24H | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1990 | ≥25 | 175-191 | 22-24 | 800 | 350 | -0.025 | -0.20 | |
YXG-26H | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1990 | ≥25 | 191-207 | 24-26 | 800 | 350 | -0.030 | -0.20 | |
YXG-28H | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1990 | ≥25 | 207-220 | 26-28 | 800 | 350 | -0.035 | -0.20 | |
YXG-30H | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1990 | ≥25 | 220-240 | 28-30 | 800 | 350 | -0.035 | -0.20 | |
YXG-32H | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1990 | ≥25 | 230-255 | 29-32 | 800 | 350 | -0.035 | -0.20 | |
YXG-22 | 0.93-0.97 | 9.3-9.7 | 676-740 | 8.5-9.3 | ≥1433 | ≥18 | 160-183 | 20-23 | 800 | 300 | -0.020 | -0.20 | |
YXG-24 | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1433 | ≥18 | 175-191 | 22-24 | 800 | 300 | -0.025 | -0.20 | |
YXG-26 | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1433 | ≥18 | 191-207 | 24-26 | 800 | 300 | -0.030 | -0.20 | |
YXG-28 | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1433 | ≥18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |
YXG-30 | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1433 | ≥18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |
YXG-32 | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1433 | ≥18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |
YXG-26M | 1.02-1.05 | 10.2-10.5 | 676-780 | 8.5-9.8 | 955-1433 | 12-18 | 191-207 | 24-26 | 800 | 300 | -0.035 | -0.20 | |
YXG-28M | 1.03-1.08 | 10.3-10.8 | 676-796 | 8.5-10.0 | 955-1433 | 12-18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |
YXG-30M | 1.08-1.10 | 10.8-11.0 | 676-835 | 8.5-10.5 | 955-1433 | 12-18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |
YXG-32M | 1.10-1.13 | 11.0-11.3 | 676-852 | 8.5-10.7 | 955-1433 | 12-18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |
YXG-24L | 0.95-1.02 | 9.5-10.2 | 541-716 | 6.8-9.0 | 636-955 | 8-12 | 175-191 | 22-24 | 800 | 250 | -0.025 | -0.20 | |
YXG-26L | 1.02-1.05 | 10.2-10.5 | 541-748 | 6.8-9.4 | 636-955 | 8-12 | 191-207 | 24-26 | 800 | 250 | -0.035 | -0.20 | |
YXG-28L | 1.03-1.08 | 10.3-10.8 | 541-764 | 6.8-9.6 | 636-955 | 8-12 | 207-220 | 26-28 | 800 | 250 | -0.035 | -0.20 | |
YXG-30L | 1.08-1.15 | 10.8-11.5 | 541-796 | 6.8-10.0 | 636-955 | 8-12 | 220-240 | 28-30 | 800 | 250 | -0.035 | -0.20 | |
YXG-32L | 1.10-1.15 | 11.0-11.5 | 541-812 | 6.8-10.2 | 636-955 | 8-12 | 230-255 | 29-32 | 800 | 250 | -0.035 | -0.20 | |
LTC(YXG-22) | 0.94-0.98 | 9.4-9.8 | 668-716 | 8.4-9.0 | ≥1433 | ≥18 | 167-183 | 21-23 | 840 | 300 | Temp Range | Br Temp Coefficient%℃ | |
–50-25℃ | ﹢0.005%℃ | ||||||||||||
20-100℃ | -0.008%℃ | ||||||||||||
100-200℃ | -0.008%℃ | ||||||||||||
200-300℃ | -0.011%℃ |
Parameter Name | Unit | SmCo5 | Sm2Co17 |
Density | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
Curie Temperature | ℃ | 700 ~ 750 | 800 ~ 850 |
Max. Operating Temperature 250 350 | ℃ | 250 | 350 |
Temperature Coefficient Of Br -0.05 -0.03 | %/℃ | -0.05 | -0.03 |
Vickers Hardness 450 ~ 500 550 ~600 | HV | 450 ~ 500 | 550 ~600 |
Electronic Ressistivity | Ω.cm | 5 ~ 6 x 10(-5) | 8 ~ 9 x 10(-5) |
Thermal Conductivity | W/mK | 12 | 13 |
UNMAG Samarium Cobalt Magnets, also known as rare earth magnets, are manufactured in China with Grade YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32. UNMAG Samarium-Cobalt Magnet can be magnetized through axial, thickness or customized as required. Its material is samarium cobalt, and it is uncoated. The delivery time is 25-30 days. It is widely used in spaceflight, national defense, microwave and sensors.
UNMAG is a leading manufacturer of Rare Earth Magnets, including Samarium Cobalt Magnets. Our Samarium Cobalt Magnets are made with the highest quality materials and are expertly crafted to meet your specific requirements. Our Samarium Cobalt Magnets are highly reliable and have a long service life.
For your Samarium Cobalt Magnet needs, trust only UNMAG. Contact us today to get started.